Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A5 | 20.0 °C | 35 % Show Material materials with Elongación A5 of 35 % |
Límite elástico Rp 0,2 | 20.0 °C | 175 - 205 MPa Show Material materials with Límite elástico Rp 0,2 of 175 - 205 MPa |
Resistencia a la tracción | 20.0 °C | 520 - 590 MPa Show Material materials with Resistencia a la tracción of 520 - 590 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.05 % Show Material materials with Carbono of 0.05 % |
Cobre | 0.5 % Show Material materials with Cobre of 0.5 % |
Cromo | 27 - 31 % Show Material materials with Cromo of 27 - 31 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Hierro | 7 - 11 % Show Material materials with Hierro of 7 - 11 % |
Manganeso | 0.5 % Show Material materials with Manganeso of 0.5 % |
Níquel | 58 % Show Material materials with Níquel of 58 % |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % |
Technological properties
Property | ||
---|---|---|
Processing history | hot-finished, annealed |