Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A5 | 20.0 °C | 30 % Show Material materials with Elongación A5 of 30 % |
Límite elástico Rp 0,2 | 20.0 °C | 175 MPa Show Material materials with Límite elástico Rp 0,2 of 175 MPa |
Resistencia a la tracción | 20.0 °C | 450 MPa Show Material materials with Resistencia a la tracción of 450 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.15 - 0.6 % Show Material materials with Aluminio of 0.15 - 0.6 % |
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.1 % Show Material materials with Carbono of 0.1 % |
Cobre | 0.75 % Show Material materials with Cobre of 0.75 % |
Cromo | 19 - 23 % Show Material materials with Cromo of 19 - 23 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Hierro | 37.4 - 50.7 % Show Material materials with Hierro of 37.4 - 50.7 % |
Manganeso | 1.5 % Show Material materials with Manganeso of 1.5 % |
Níquel | 30 - 35 % Show Material materials with Níquel of 30 - 35 % |
Silicona | 1 % Show Material materials with Silicona of 1 % |
Titanio | 0.15 - 0.6 % Show Material materials with Titanio of 0.15 - 0.6 % |
Technological properties
Property | ||
---|---|---|
Processing history | hot-finished, annealed |