General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Dureza Brinell | 23.0 °C | 121 - 240 [-] Show Material materials with Dureza Brinell of 121 - 240 [-] | |
Dureza Rockwell B | 23.0 °C | 69 - 103 [-] Show Material materials with Dureza Rockwell B of 69 - 103 [-] | |
Dureza Rockwell C | 23.0 °C | 22 - 28 [-] Show Material materials with Dureza Rockwell C of 22 - 28 [-] | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 23.0 °C | 450 - 850 MPa Show Material materials with Resistencia a la tracción of 450 - 850 MPa |