General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Elongación A50 | 23.0 °C | 38 % Show Material materials with Elongación A50 of 38 % | |
Elongación A80 | 23.0 °C | 38 % Show Material materials with Elongación A80 of 38 % | |
Límite elástico | 23.0 °C | 120 MPa Show Material materials with Límite elástico of 120 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 23.0 °C | 350 MPa Show Material materials with Resistencia a la tracción of 350 MPa |