General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 20.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for High Carbon Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for High Carbon Steel |
Dureza Brinell | 20.0 °C | 167 [-] Show Material materials with Dureza Brinell of 167 [-] | |
Elongación A5 | 20.0 °C | 18 % Show Material materials with Elongación A5 of 18 % | |
Elongación A5 transversal | 20.0 °C | 14 % Show Material materials with Elongación A5 transversal of 14 % | |
Estricción | 20.0 °C | 35 % Show Material materials with Estricción of 35 % | |
Límite elástico | 20.0 °C | 295 MPa Show Material materials with Límite elástico of 295 MPa | |
Módulo de cizallamiento | 20.0 °C | 75 - 80 GPa Show Material materials with Módulo de cizallamiento of 75 - 80 GPa | Typical for Carbon Steel |
Módulo elástico | 20.0 °C | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for High Carbon Steel |
Reducción de área, transversal | 20.0 °C | 26 % Show Material materials with Reducción de área, transversal of 26 % | |
Resistencia a la tracción | 20.0 °C | 590 - 690 MPa Show Material materials with Resistencia a la tracción of 590 - 690 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 20.0 °C | 1.32E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.32E-5 1/K | Typical for High Carbon Steel |
Temperatura de fusión | 1289 - 1478 °C Show Material materials with Temperatura de fusión of 1289 - 1478 °C | Typical for High Carbon Steel | |
Temperatura máx. de funcionamiento | 500 °C Show Material materials with Temperatura máx. de funcionamiento of 500 °C | Typical for Carbon Steel |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 20.0 °C | 1.43E-7 - 1.74E-7 Ω·m Show Material materials with Resistividad eléctrica of 1.43E-7 - 1.74E-7 Ω·m | Typical for Carbon Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.035 % Show Material materials with Azufre of 0.035 % |
Carbono | 0.6 % Show Material materials with Carbono of 0.6 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Hierro | 97.63 - 99.55 % Show Material materials with Hierro of 97.63 - 99.55 % |
Manganeso | 0.3 - 1.2 % Show Material materials with Manganeso of 0.3 - 1.2 % |
Silicona | 0.15 - 0.5 % Show Material materials with Silicona of 0.15 - 0.5 % |
Technological properties
Property | ||
---|---|---|
Processing history | annealed, normalized or normalized and tempered |