General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Dureza Brinell | 23.0 °C | 277 - 311 [-] Show Material materials with Dureza Brinell of 277 - 311 [-] | |
Elongación A5 | 23.0 °C | 12 - 15 % Show Material materials with Elongación A5 of 12 - 15 % | |
Estricción | 23.0 °C | 45 - 50 % Show Material materials with Estricción of 45 - 50 % | |
Límite elástico Rp 0,2 | 23.0 °C | 725 - 860 MPa Show Material materials with Límite elástico Rp 0,2 of 725 - 860 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 23.0 °C | 930 - 1000 MPa Show Material materials with Resistencia a la tracción of 930 - 1000 MPa | |
Resistencia al choque, ensayo Charpy entallado | 20.0 °C | 27 - 41 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 27 - 41 kJ/m² |