General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Dureza Brinell | 23.0 °C | 192 [-] Show Material materials with Dureza Brinell of 192 [-] | |
Dureza Rockwell B | 23.0 °C | 90 [-] Show Material materials with Dureza Rockwell B of 90 [-] | |
Dureza Vickers | 23.0 °C | 200 [-] Show Material materials with Dureza Vickers of 200 [-] | |
Elongación A5 | 23.0 °C | 20 % Show Material materials with Elongación A5 of 20 % | |
Límite elástico Rp 0,2 | 23.0 °C | 245 MPa Show Material materials with Límite elástico Rp 0,2 of 245 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 23.0 °C | 410 MPa Show Material materials with Resistencia a la tracción of 410 MPa |
Technological properties
Property | ||
---|---|---|
Processing history | annealed |