Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A5 | 20.0 °C | 8 - 10 % Show Material materials with Elongación A5 of 8 - 10 % |
Estricción | 20.0 °C | 60 % Show Material materials with Estricción of 60 % |
Resistencia a la tracción | 20.0 °C | 600 - 830 MPa Show Material materials with Resistencia a la tracción of 600 - 830 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.35 % Show Material materials with Aluminio of 0.35 % |
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Boro | 0.001 - 0.01 % Show Material materials with Boro of 0.001 - 0.01 % |
Carbono | 0.08 % Show Material materials with Carbono of 0.08 % |
Cromo | 13.5 - 16 % Show Material materials with Cromo of 13.5 - 16 % |
Fósforo | 0.05 % Show Material materials with Fósforo of 0.05 % |
Hierro | 49.13 - 59.5 % Show Material materials with Hierro of 49.13 - 59.5 % |
Manganeso | 2 % Show Material materials with Manganeso of 2 % |
Molibdeno | 1 - 1.5 % Show Material materials with Molibdeno of 1 - 1.5 % |
Níquel | 24 - 27 % Show Material materials with Níquel of 24 - 27 % |
Silicona | 1 % Show Material materials with Silicona of 1 % |
Titanio | 1.9 % Show Material materials with Titanio of 1.9 % |
Vanadio | 0.1 - 0.5 % Show Material materials with Vanadio of 0.1 - 0.5 % |