Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A5 | 20.0 °C | 20 - 25 % Show Material materials with Elongación A5 of 20 - 25 % |
Estricción | 20.0 °C | 65 % Show Material materials with Estricción of 65 % |
Resistencia a la tracción | 20.0 °C | 450 - 680 MPa Show Material materials with Resistencia a la tracción of 450 - 680 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.08 % Show Material materials with Carbono of 0.08 % |
Cobre | 3 - 4 % Show Material materials with Cobre of 3 - 4 % |
Cromo | 17 - 19 % Show Material materials with Cromo of 17 - 19 % |
Fósforo | 0.05 % Show Material materials with Fósforo of 0.05 % |
Hierro | 63.34 - 71.5 % Show Material materials with Hierro of 63.34 - 71.5 % |
Manganeso | 2 % Show Material materials with Manganeso of 2 % |
Níquel | 8.5 - 10.5 % Show Material materials with Níquel of 8.5 - 10.5 % |
Silicona | 1 % Show Material materials with Silicona of 1 % |