General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Medium Carbon Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Medium Carbon Steel |
Dureza Rockwell B | 23.0 °C | 85 [-] Show Material materials with Dureza Rockwell B of 85 [-] | |
Dureza Vickers | 23.0 °C | 180 [-] Show Material materials with Dureza Vickers of 180 [-] | |
Elongación A50 | 23.0 °C | 15 % Show Material materials with Elongación A50 of 15 % | |
Elongación A80 | 23.0 °C | 13 % Show Material materials with Elongación A80 of 13 % | |
Hardness, Rockwell Superficial 15-T | 23.0 °C | 88 [-] Show Material materials with Hardness, Rockwell Superficial 15-T of 88 [-] | |
Hardness, Rockwell Superficial 30-T | 23.0 °C | 73 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 73 [-] | |
Módulo de cizallamiento | 23.0 °C | 75 - 80 GPa Show Material materials with Módulo de cizallamiento of 75 - 80 GPa | Typical for Carbon Steel |
Módulo elástico | 23.0 °C | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Medium Carbon Steel |
Resistencia a la tracción | 23.0 °C | 610 MPa Show Material materials with Resistencia a la tracción of 610 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 470 - 520 J/(kg·K) Show Material materials with Calor específico of 470 - 520 J/(kg·K) | Typical for Medium Carbon Steel |
Coeficiente de dilatación térmica | 23.0 °C | 1.32E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.32E-5 1/K | Typical for Medium Carbon Steel |
Conductividad térmica | 23.0 °C | 21 - 52 W/(m·K) Show Material materials with Conductividad térmica of 21 - 52 W/(m·K) | Typical for Medium Carbon Steel |
Temperatura de fusión | 1380 - 1514 °C Show Material materials with Temperatura de fusión of 1380 - 1514 °C | Typical for Medium Carbon Steel | |
Temperatura máx. de funcionamiento | 500 °C Show Material materials with Temperatura máx. de funcionamiento of 500 °C | Typical for Carbon Steel |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 23.0 °C | 1.43E-7 - 1.74E-7 Ω·m Show Material materials with Resistividad eléctrica of 1.43E-7 - 1.74E-7 Ω·m | Typical for Carbon Steel |
Technological properties
Property | ||
---|---|---|
Processing history | annealed |