Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 269 [-] Show Material materials with Dureza Brinell of 269 [-] |
Chemical properties
Property | Value |
---|---|
Aluminio | 1 - 1.8 % Show Material materials with Aluminio of 1 - 1.8 % |
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.04 - 0.1 % Show Material materials with Carbono of 0.04 - 0.1 % |
Cobre | 0.2 % Show Material materials with Cobre of 0.2 % |
Cromo | 18 - 21 % Show Material materials with Cromo of 18 - 21 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Hierro | 1.5 % Show Material materials with Hierro of 1.5 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Silicona | 1 % Show Material materials with Silicona of 1 % |
Titanio | 1.8 - 2.7 % Show Material materials with Titanio of 1.8 - 2.7 % |
Technological properties
Property | ||
---|---|---|
Processing history | solution treated |