Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 241 - 269 [-] Show Material materials with Dureza Brinell of 241 - 269 [-] |
Dureza Rockwell B | 20.0 °C | 100 [-] Show Material materials with Dureza Rockwell B of 100 [-] |
Dureza Rockwell C | 20.0 °C | 27 [-] Show Material materials with Dureza Rockwell C of 27 [-] |
Dureza Vickers | 20.0 °C | 250 - 285 [-] Show Material materials with Dureza Vickers of 250 - 285 [-] |
Elongación A5 | 20.0 °C | 15 - 25 % Show Material materials with Elongación A5 of 15 - 25 % |
Límite elástico Rp 0,2 | 20.0 °C | 615 - 635 MPa Show Material materials with Límite elástico Rp 0,2 of 615 - 635 MPa |
Resistencia a la tracción | 20.0 °C | 1000 - 1030 MPa Show Material materials with Resistencia a la tracción of 1000 - 1030 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 1 - 1.8 % Show Material materials with Aluminio of 1 - 1.8 % |
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.04 - 0.1 % Show Material materials with Carbono of 0.04 - 0.1 % |
Cobre | 0.2 % Show Material materials with Cobre of 0.2 % |
Cromo | 18 - 21 % Show Material materials with Cromo of 18 - 21 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Hierro | 1.5 % Show Material materials with Hierro of 1.5 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Silicona | 1 % Show Material materials with Silicona of 1 % |
Titanio | 1.8 - 2.7 % Show Material materials with Titanio of 1.8 - 2.7 % |
Technological properties
Property | ||
---|---|---|
Processing history | ageing treatment after solution treatment |