Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 260 [-] Show Material materials with Dureza Brinell of 260 [-] |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.05 % Show Material materials with Aluminio of 0.05 % |
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.85 - 1 % Show Material materials with Carbono of 0.85 - 1 % |
Cobre | 0.3 % Show Material materials with Cobre of 0.3 % |
Cromo | 1.4 - 1.8 % Show Material materials with Cromo of 1.4 - 1.8 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 1.4 - 1.7 % Show Material materials with Manganeso of 1.4 - 1.7 % |
Molibdeno | 0.1 % Show Material materials with Molibdeno of 0.1 % |
Níquel | 0.25 % Show Material materials with Níquel of 0.25 % |
Oxígeno | 1.5E-3 % Show Material materials with Oxígeno of 1.5E-3 % |
Silicona | 0.5 - 0.8 % Show Material materials with Silicona of 0.5 - 0.8 % |
Titanio | 5E-3 % Show Material materials with Titanio of 5E-3 % |