General
Property | Value | Comment |
---|---|---|
Densidad | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Low Carbon Steel |
Mecánica
Property | Value | Comment |
---|---|---|
Coeficiente de Poisson | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Low Carbon Steel |
Elongación | 15.0 % Show Material materials with Elongación of 15.0 % | Predicted Value, A200 |
15.4 % Show Material materials with Elongación of 15.4 % | Predicted Value, A80 | |
18.3 % Show Material materials with Elongación of 18.3 % | Predicted Value, Transverse | |
20.2 % Show Material materials with Elongación of 20.2 % | Predicted Value, A80 Transverse | |
20.6 % Show Material materials with Elongación of 20.6 % | Predicted Value, A5 | |
21 % Show Material materials with Elongación of 21 % | Predicted Value, A50 | |
21.6 % Show Material materials with Elongación of 21.6 % | Predicted Value | |
Estricción | 42.1 % Show Material materials with Estricción of 42.1 % | Predicted Value |
43.0 % Show Material materials with Estricción of 43.0 % | Predicted Value, Transverse | |
Módulo de cizallamiento | 82 GPa Show Material materials with Módulo de cizallamiento of 82 GPa | Typical for Low Carbon Steel |
Módulo elástico | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Low Carbon Steel |
Resistencia al cizallamiento | 511.2 MPa Show Material materials with Resistencia al cizallamiento of 511.2 MPa | Predicted Value |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 465 J/(kg·K) Show Material materials with Calor específico of 465 J/(kg·K) | Typical for Low Carbon Steel |
Coeficiente de dilatación térmica | 1.32e-05 - 1.38e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.32e-05 - 1.38e-05 1/K | Typical for Low Carbon Steel |
Conductividad térmica | 25 - 93 W/(m·K) Show Material materials with Conductividad térmica of 25 - 93 W/(m·K) | Typical for Low Carbon Steel |
Temperatura de fusión | 1480 - 1526 °C Show Material materials with Temperatura de fusión of 1480 - 1526 °C | Typical for Low Carbon Steel |
Temperatura máx. de funcionamiento | 315.4 °C Show Material materials with Temperatura máx. de funcionamiento of 315.4 °C | Predicted Value, Long |
500 °C Show Material materials with Temperatura máx. de funcionamiento of 500 °C | Typical for Carbon Steel |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 7 S/m Show Material materials with Conductividad eléctrica of 7 S/m | Predicted Value |
Resistividad eléctrica | 1.43e-07 - 1.74e-07 Ω·m Show Material materials with Resistividad eléctrica of 1.43e-07 - 1.74e-07 Ω·m | Typical for Carbon Steel |
Magnético
Property | Value | Comment |
---|---|---|
Temperatura de Curie | 770 °C Show Material materials with Temperatura de Curie of 770 °C | Typical for Low Carbon Steel |
Chemical properties
Property | Value | Related Standards |
---|---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % | ASTM A573 |
Carbono | 0.23 % Show Material materials with Carbono of 0.23 % | ASTM A573 |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % | ASTM A573 |
Manganeso | 0.6 - 0.9 % Show Material materials with Manganeso of 0.6 - 0.9 % | ASTM A573 |
Silicona | 0.1 - 0.35 % Show Material materials with Silicona of 0.1 - 0.35 % | ASTM A573 |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |