General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 20.0 °C | 7.85 g/cm³ Show Material materials with Densidad of 7.85 g/cm³ | Typical for Carbon Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Carbon Steel |
Elongación A50 | 20.0 °C | 21 % Show Material materials with Elongación A50 of 21 % | |
Elongation A200 | 20.0 °C | 17 % Show Material materials with Elongation A200 of 17 % | |
Límite elástico | 20.0 °C | 260 MPa Show Material materials with Límite elástico of 260 MPa | |
Módulo de cizallamiento | 20.0 °C | 75 - 80 GPa Show Material materials with Módulo de cizallamiento of 75 - 80 GPa | Typical for Carbon Steel |
Resistencia a la tracción | 20.0 °C | 485 - 620 MPa Show Material materials with Resistencia a la tracción of 485 - 620 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 20.0 °C | 1.2E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.2E-5 1/K | Typical for Carbon Steel |
Temperatura de fusión | 1425 - 1540 °C Show Material materials with Temperatura de fusión of 1425 - 1540 °C | Typical for Carbon Steel | |
Temperatura máx. de funcionamiento | 500 °C Show Material materials with Temperatura máx. de funcionamiento of 500 °C | Typical for Carbon Steel |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 20.0 °C | 1.43E-7 - 1.74E-7 Ω·m Show Material materials with Resistividad eléctrica of 1.43E-7 - 1.74E-7 Ω·m | Typical for Carbon Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % |
Carbono | 0.31 % Show Material materials with Carbono of 0.31 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 1.2 % Show Material materials with Manganeso of 1.2 % |
Silicona | 0.15 - 0.4 % Show Material materials with Silicona of 0.15 - 0.4 % |