Mecánica
Property | Temperature | Value |
---|---|---|
Estricción | 23.0 °C | 40 - 45 % Show Material materials with Estricción of 40 - 45 % |
Resistencia a la tracción | 23.0 °C | 1450 - 2030 MPa Show Material materials with Resistencia a la tracción of 1450 - 2030 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % |
Carbono | 0.6 - 0.7 % Show Material materials with Carbono of 0.6 - 0.7 % |
Cromo | 0.35 - 0.6 % Show Material materials with Cromo of 0.35 - 0.6 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.5 - 0.9 % Show Material materials with Manganeso of 0.5 - 0.9 % |
Silicona | 0.15 - 0.3 % Show Material materials with Silicona of 0.15 - 0.3 % |
Vanadio | 0.1 - 0.25 % Show Material materials with Vanadio of 0.1 - 0.25 % |