Mecánica
Property | Temperature | Value |
---|---|---|
Estricción | 23.0 °C | 30 - 40 % Show Material materials with Estricción of 30 - 40 % |
Resistencia a la tracción | 23.0 °C | 1690 - 2370 MPa Show Material materials with Resistencia a la tracción of 1690 - 2370 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % |
Carbono | 0.55 - 0.68 % Show Material materials with Carbono of 0.55 - 0.68 % |
Cromo | 0.5 - 0.8 % Show Material materials with Cromo of 0.5 - 0.8 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.5 - 0.9 % Show Material materials with Manganeso of 0.5 - 0.9 % |
Silicona | 1.2 - 1.65 % Show Material materials with Silicona of 1.2 - 1.65 % |
Vanadio | 0.08 - 0.25 % Show Material materials with Vanadio of 0.08 - 0.25 % |