General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Chromium Molybdenum Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Chromium Molybdenum Steel |
Dureza Brinell | 23.0 °C | 255 - 302 [-] Show Material materials with Dureza Brinell of 255 - 302 [-] | |
Elongación A50 | 23.0 °C | 15 % Show Material materials with Elongación A50 of 15 % | |
Energía de impacto Charpy | 23.0 °C | 11 J Show Material materials with Energía de impacto Charpy of 11 J | |
Estricción | 23.0 °C | 40 % Show Material materials with Estricción of 40 % | |
Límite elástico Rp 0,2 | 23.0 °C | 585 MPa Show Material materials with Límite elástico Rp 0,2 of 585 MPa | |
Módulo elástico | 23.0 °C | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Chromium Molybdenum Steel |
Resistencia a la tracción | 23.0 °C | 825 MPa Show Material materials with Resistencia a la tracción of 825 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 448 - 502 J/(kg·K) Show Material materials with Calor específico of 448 - 502 J/(kg·K) | Typical for Chromium Molybdenum Steel |
Coeficiente de dilatación térmica | 23.0 °C | 1.1E-5 - 1.4E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.1E-5 - 1.4E-5 1/K | Typical for Chromium Molybdenum Steel |
Conductividad térmica | 23.0 °C | 36 - 43 W/(m·K) Show Material materials with Conductividad térmica of 36 - 43 W/(m·K) | Typical for Chromium Molybdenum Steel |
Temperatura de fusión | 1382 - 1529 °C Show Material materials with Temperatura de fusión of 1382 - 1529 °C | Typical for Chromium Molybdenum Steel |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.85 - 1.3 % Show Material materials with Aluminio of 0.85 - 1.3 % |
Azufre | 0.04 % Show Material materials with Azufre of 0.04 % |
Carbono | 0.38 - 0.45 % Show Material materials with Carbono of 0.38 - 0.45 % |
Cobre | 0.35 % Show Material materials with Cobre of 0.35 % |
Cromo | 1.4 - 1.8 % Show Material materials with Cromo of 1.4 - 1.8 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 0.4 - 0.7 % Show Material materials with Manganeso of 0.4 - 0.7 % |
Molibdeno | 0.3 - 0.45 % Show Material materials with Molibdeno of 0.3 - 0.45 % |
Níquel | 0.3 % Show Material materials with Níquel of 0.3 % |
Silicona | 0.4 % Show Material materials with Silicona of 0.4 % |
Vanadio | 0.03 % Show Material materials with Vanadio of 0.03 % |