General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Elongación A50 | 23.0 °C | 22 % Show Material materials with Elongación A50 of 22 % | |
Energía de impacto Charpy | 23.0 °C | 18 J Show Material materials with Energía de impacto Charpy of 18 J | |
Límite elástico | 23.0 °C | 450 MPa Show Material materials with Límite elástico of 450 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 23.0 °C | 550 MPa Show Material materials with Resistencia a la tracción of 550 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.06 % Show Material materials with Aluminio of 0.06 % |
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.2 % Show Material materials with Carbono of 0.2 % |
Cobre | 0.15 % Show Material materials with Cobre of 0.15 % |
Cromo | 0.15 % Show Material materials with Cromo of 0.15 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 1.15 - 1.5 % Show Material materials with Manganeso of 1.15 - 1.5 % |
Molibdeno | 0.05 % Show Material materials with Molibdeno of 0.05 % |
Niobio | 0.05 % Show Material materials with Niobio of 0.05 % |
Níquel | 0.25 % Show Material materials with Níquel of 0.25 % |
Silicona | 0.1 - 0.35 % Show Material materials with Silicona of 0.1 - 0.35 % |
Vanadio | 0.12 % Show Material materials with Vanadio of 0.12 % |