Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A50 | 23.0 °C | 16.5 - 30 % Show Material materials with Elongación A50 of 16.5 - 30 % |
Energía de impacto Charpy | 23.0 °C | 18 J Show Material materials with Energía de impacto Charpy of 18 J |
Límite elástico | 23.0 °C | 240 MPa Show Material materials with Límite elástico of 240 MPa |
Resistencia a la tracción | 23.0 °C | 415 MPa Show Material materials with Resistencia a la tracción of 415 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.04 - 0.3 % Show Material materials with Aluminio of 0.04 - 0.3 % |
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % |
Carbono | 0.12 % Show Material materials with Carbono of 0.12 % |
Cobre | 0.4 - 0.75 % Show Material materials with Cobre of 0.4 - 0.75 % |
Cromo | 0.44 - 1.01 % Show Material materials with Cromo of 0.44 - 1.01 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.5 - 1.05 % Show Material materials with Manganeso of 0.5 - 1.05 % |
Níquel | 0.47 - 0.98 % Show Material materials with Níquel of 0.47 - 0.98 % |
Silicona | 0.08 - 0.37 % Show Material materials with Silicona of 0.08 - 0.37 % |