Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 163 [-] Show Material materials with Dureza Brinell of 163 [-] |
Dureza Rockwell B | 23.0 °C | 85 [-] Show Material materials with Dureza Rockwell B of 85 [-] |
Elongación A50 | 23.0 °C | 35 % Show Material materials with Elongación A50 of 35 % |
Límite elástico | 23.0 °C | 205 MPa Show Material materials with Límite elástico of 205 MPa |
Resistencia a la tracción | 23.0 °C | 380 MPa Show Material materials with Resistencia a la tracción of 380 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % |
Carbono | 0.3 % Show Material materials with Carbono of 0.3 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.4 - 1.06 % Show Material materials with Manganeso of 0.4 - 1.06 % |