Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 190 [-] Show Material materials with Dureza Brinell of 190 [-] |
Dureza Rockwell B | 23.0 °C | 90 [-] Show Material materials with Dureza Rockwell B of 90 [-] |
Elongación A50 | 23.0 °C | 30 % Show Material materials with Elongación A50 of 30 % |
Límite elástico | 23.0 °C | 240 MPa Show Material materials with Límite elástico of 240 MPa |
Resistencia a la tracción | 23.0 °C | 450 MPa Show Material materials with Resistencia a la tracción of 450 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % |
Carbono | 0.19 % Show Material materials with Carbono of 0.19 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.31 - 0.64 % Show Material materials with Manganeso of 0.31 - 0.64 % |
Níquel | 3.18 - 3.82 % Show Material materials with Níquel of 3.18 - 3.82 % |
Silicona | 0.18 - 0.37 % Show Material materials with Silicona of 0.18 - 0.37 % |