Chemical properties
Property | Value |
---|---|
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % |
Carbono | 0.2 % Show Material materials with Carbono of 0.2 % |
Cobre | 0.75 - 1.25 % Show Material materials with Cobre of 0.75 - 1.25 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.4 - 1.06 % Show Material materials with Manganeso of 0.4 - 1.06 % |
Níquel | 1.6 - 2.24 % Show Material materials with Níquel of 1.6 - 2.24 % |