General
Property | Value | Comment |
---|---|---|
Densidad | 8.8 g/cm³ Show Material materials with Densidad of 8.8 g/cm³ | Typical for Nickel Steel |
Mecánica
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coeficiente de Poisson | 0.291 [-] Show Material materials with Coeficiente de Poisson of 0.291 [-] | Typical for Nickel Steel | |||
Elongación | 16.4 % Show Material materials with Elongación of 16.4 % | Predicted Value, A200 | |||
18.4 % Show Material materials with Elongación of 18.4 % | Predicted Value, Transverse | ||||
20 % Show Material materials with Elongación of 20 % | Double-Normalized and Tempered | ASTM A353 | Plate | A50 | |
21.1 % Show Material materials with Elongación of 21.1 % | Predicted Value | ||||
22.2 % Show Material materials with Elongación of 22.2 % | Predicted Value, A80 | ||||
29.0 % Show Material materials with Elongación of 29.0 % | Predicted Value, A80 Transverse | ||||
Estricción | 42.6 % Show Material materials with Estricción of 42.6 % | Predicted Value, Transverse | |||
44.7 % Show Material materials with Estricción of 44.7 % | Predicted Value | ||||
Módulo de cizallamiento | 76 GPa Show Material materials with Módulo de cizallamiento of 76 GPa | Typical for Nickel Steel | |||
Módulo elástico | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Nickel Steel | |||
Resistencia a la tracción | 690 - 825 MPa Show Material materials with Resistencia a la tracción of 690 - 825 MPa | Double-Normalized and Tempered | ASTM A353 | Plate | |
Resistencia al cizallamiento | 581.2 MPa Show Material materials with Resistencia al cizallamiento of 581.2 MPa | Predicted Value |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 456 J/(kg·K) Show Material materials with Calor específico of 456 J/(kg·K) | Typical for Nickel Steel |
Coeficiente de dilatación térmica | 12.25 1/K Show Material materials with Coeficiente de dilatación térmica of 12.25 1/K | Predicted Value |
Conductividad térmica | 10 - 50 W/(m·K) Show Material materials with Conductividad térmica of 10 - 50 W/(m·K) | Typical for Nickel Steel |
Temperatura de fusión | 1316 - 1595 °C Show Material materials with Temperatura de fusión of 1316 - 1595 °C | Typical for Nickel Steel |
Eléctrico
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % | Double-Normalized and Tempered | ASTM A353 | Plate |
Carbono | 0.13 % Show Material materials with Carbono of 0.13 % | Double-Normalized and Tempered | ASTM A353 | Plate |
Fósforo | 0.015 % Show Material materials with Fósforo of 0.015 % | Double-Normalized and Tempered | ASTM A353 | Plate |
Manganeso | 0.9 % Show Material materials with Manganeso of 0.9 % | Double-Normalized and Tempered | ASTM A353 | Plate |
Níquel | 8.5 - 9.5 % Show Material materials with Níquel of 8.5 - 9.5 % | Double-Normalized and Tempered | ASTM A353 | Plate |
Silicona | 0.15 - 0.4 % Show Material materials with Silicona of 0.15 - 0.4 % | Double-Normalized and Tempered | ASTM A353 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |