Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 156 [-] Show Material materials with Dureza Brinell of 156 [-] |
Elongación A50 | 20.0 °C | 18 % Show Material materials with Elongación A50 of 18 % |
Resistencia a la tracción | 20.0 °C | 515 - 690 MPa Show Material materials with Resistencia a la tracción of 515 - 690 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 310 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 310 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.01 % Show Material materials with Azufre of 0.01 % |
Carbono | 0.35 % Show Material materials with Carbono of 0.35 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Manganeso | 1.35 % Show Material materials with Manganeso of 1.35 % |
Silicona | 0.15 - 0.35 % Show Material materials with Silicona of 0.15 - 0.35 % |