General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Dureza Brinell | 23.0 °C | 248 [-] Show Material materials with Dureza Brinell of 248 [-] | |
Elongación A50 | 23.0 °C | 16 % Show Material materials with Elongación A50 of 16 % | |
Límite elástico Rp 0,2 | 23.0 °C | 690 MPa Show Material materials with Límite elástico Rp 0,2 of 690 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 23.0 °C | 795 - 965 MPa Show Material materials with Resistencia a la tracción of 795 - 965 MPa |
Chemical properties
Property | Value |
---|---|
Carbono | 0.4 % Show Material materials with Carbono of 0.4 % |
Cromo | 2.3 - 3.3 % Show Material materials with Cromo of 2.3 - 3.3 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Manganeso | 0.9 % Show Material materials with Manganeso of 0.9 % |
Molibdeno | 0.8 - 2 % Show Material materials with Molibdeno of 0.8 - 2 % |
Níquel | 0.35 % Show Material materials with Níquel of 0.35 % |
Silicona | 0.02 % Show Material materials with Silicona of 0.02 % |
Vanadio | 0.3 - 0.5 % Show Material materials with Vanadio of 0.3 - 0.5 % |