Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A50 | 20.0 °C | 40 % Show Material materials with Elongación A50 of 40 % |
Estricción | 20.0 °C | 50 % Show Material materials with Estricción of 50 % |
Resistencia a la tracción | 20.0 °C | 500 MPa Show Material materials with Resistencia a la tracción of 500 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 214 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 214 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.02 % Show Material materials with Carbono of 0.02 % |
Cobre | 0.6 - 1.4 % Show Material materials with Cobre of 0.6 - 1.4 % |
Cromo | 26 - 28 % Show Material materials with Cromo of 26 - 28 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 2 % Show Material materials with Manganeso of 2 % |
Molibdeno | 4 - 5 % Show Material materials with Molibdeno of 4 - 5 % |
Níquel | 30 - 34 % Show Material materials with Níquel of 30 - 34 % |
Silicona | 0.6 % Show Material materials with Silicona of 0.6 % |