Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A50 | 23.0 °C | 30 % Show Material materials with Elongación A50 of 30 % |
Estricción | 23.0 °C | 50 % Show Material materials with Estricción of 50 % |
Límite elástico Rp 0,2 | 23.0 °C | 310 MPa Show Material materials with Límite elástico Rp 0,2 of 310 MPa |
Resistencia a la tracción | 23.0 °C | 655 MPa Show Material materials with Resistencia a la tracción of 655 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.03 % Show Material materials with Carbono of 0.03 % |
Cobre | 0.75 % Show Material materials with Cobre of 0.75 % |
Cromo | 20 - 22 % Show Material materials with Cromo of 20 - 22 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 2 % Show Material materials with Manganeso of 2 % |
Molibdeno | 6 - 7 % Show Material materials with Molibdeno of 6 - 7 % |
Nitrógeno | 0.18 - 0.25 % Show Material materials with Nitrógeno of 0.18 - 0.25 % |
Níquel | 23.5 - 25.5 % Show Material materials with Níquel of 23.5 - 25.5 % |
Silicona | 1 % Show Material materials with Silicona of 1 % |