Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A50 | 23.0 °C | 40 % Show Material materials with Elongación A50 of 40 % |
Estricción | 23.0 °C | 50 % Show Material materials with Estricción of 50 % |
Límite elástico Rp 0,2 | 23.0 °C | 214 MPa Show Material materials with Límite elástico Rp 0,2 of 214 MPa |
Resistencia a la tracción | 23.0 °C | 500 MPa Show Material materials with Resistencia a la tracción of 500 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.03 % Show Material materials with Carbono of 0.03 % |
Cobre | 0.6 - 1.4 % Show Material materials with Cobre of 0.6 - 1.4 % |
Cromo | 26 - 28 % Show Material materials with Cromo of 26 - 28 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 2.5 % Show Material materials with Manganeso of 2.5 % |
Molibdeno | 3 - 4 % Show Material materials with Molibdeno of 3 - 4 % |
Níquel | 30 - 34 % Show Material materials with Níquel of 30 - 34 % |
Silicona | 1 % Show Material materials with Silicona of 1 % |