Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 20.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Molybdenum Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Molybdenum Steel |
Elongación A50 | 20.0 °C | 10 % Show Material materials with Elongación A50 of 10 % | |
Elongation A200 | 20.0 °C | 7 % Show Material materials with Elongation A200 of 7 % | |
Límite elástico | 20.0 °C | 520 MPa Show Material materials with Límite elástico of 520 MPa | |
Módulo elástico | 20.0 °C | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Molybdenum Steel |
Resistencia a la tracción | 20.0 °C | 690 MPa Show Material materials with Resistencia a la tracción of 690 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 456 J/(kg·K) Show Material materials with Calor específico of 456 J/(kg·K) | Typical for Molybdenum Steel |
Coeficiente de dilatación térmica | 20.0 °C | 1.29E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.29E-5 1/K | Typical for Molybdenum Steel |
Conductividad térmica | 20.0 °C | 37 - 48 W/(m·K) Show Material materials with Conductividad térmica of 37 - 48 W/(m·K) | Typical for Molybdenum Steel |
Temperatura de fusión | 1382 - 1529 °C Show Material materials with Temperatura de fusión of 1382 - 1529 °C | Typical for Molybdenum Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.08 - 0.13 % Show Material materials with Azufre of 0.08 - 0.13 % |
Carbono | 0.32 - 0.39 % Show Material materials with Carbono of 0.32 - 0.39 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 1.35 - 1.65 % Show Material materials with Manganeso of 1.35 - 1.65 % |
Molibdeno | 0.01 - 0.3 % Show Material materials with Molibdeno of 0.01 - 0.3 % |
Niobio | 0.01 - 0.07 % Show Material materials with Niobio of 0.01 - 0.07 % |
Vanadio | 0.02 - 0.2 % Show Material materials with Vanadio of 0.02 - 0.2 % |