General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.6 - 7.8 g/cm³ Show Material materials with Densidad of 7.6 - 7.8 g/cm³ | Typical for Ferritic Stainless Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Ferritic Stainless Steel |
Dureza Brinell | 23.0 °C | 269 [-] Show Material materials with Dureza Brinell of 269 [-] | |
Elongación A50 | 23.0 °C | 18 % Show Material materials with Elongación A50 of 18 % | |
Energía de impacto Charpy | 23.0 °C | 40 J Show Material materials with Energía de impacto Charpy of 40 J | |
Estricción | 23.0 °C | 50 % Show Material materials with Estricción of 50 % | |
Límite elástico Rp 0,2 | 23.0 °C | 620 MPa Show Material materials with Límite elástico Rp 0,2 of 620 MPa | |
Módulo de cizallamiento | 23.0 °C | 77 GPa Show Material materials with Módulo de cizallamiento of 77 GPa | Typical for Ferritic Stainless Steel |
Módulo elástico | 23.0 °C | 220 GPa Show Material materials with Módulo elástico of 220 GPa | Typical for Ferritic Stainless Steel |
Resistencia a la tracción | 23.0 °C | 760 MPa Show Material materials with Resistencia a la tracción of 760 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 420 - 586 J/(kg·K) Show Material materials with Calor específico of 420 - 586 J/(kg·K) | Typical for Ferritic Stainless Steel |
Coeficiente de dilatación térmica | 23.0 °C | 9.3E-6 - 1.2E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 9.3E-6 - 1.2E-5 1/K | Typical for Ferritic Stainless Steel |
Conductividad térmica | 23.0 °C | 11 - 22 W/(m·K) Show Material materials with Conductividad térmica of 11 - 22 W/(m·K) | Typical for Ferritic Stainless Steel |
Temperatura de fusión | 1425 - 1530 °C Show Material materials with Temperatura de fusión of 1425 - 1530 °C | Typical for Ferritic Stainless Steel |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 23.0 °C | 6E-7 - 7.5E-7 Ω·m Show Material materials with Resistividad eléctrica of 6E-7 - 7.5E-7 Ω·m | Typical for Ferritic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.025 % Show Material materials with Aluminio of 0.025 % |
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.1 - 0.15 % Show Material materials with Carbono of 0.1 - 0.15 % |
Cobre | 0.15 % Show Material materials with Cobre of 0.15 % |
Cromo | 11.5 - 13 % Show Material materials with Cromo of 11.5 - 13 % |
Estaño | 0.05 % Show Material materials with Estaño of 0.05 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Manganeso | 0.25 - 0.8 % Show Material materials with Manganeso of 0.25 - 0.8 % |
Molibdeno | 0.5 % Show Material materials with Molibdeno of 0.5 % |
Niobio | 0.2 % Show Material materials with Niobio of 0.2 % |
Nitrógeno | 0.08 % Show Material materials with Nitrógeno of 0.08 % |
Níquel | 0.75 % Show Material materials with Níquel of 0.75 % |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % |
Titanio | 0.05 % Show Material materials with Titanio of 0.05 % |
Wolframio | 0.1 % Show Material materials with Wolframio of 0.1 % |