General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Dureza Brinell | 23.0 °C | 331 [-] Show Material materials with Dureza Brinell of 331 [-] | |
Elongación A50 | 23.0 °C | 13 % Show Material materials with Elongación A50 of 13 % | |
Energía de impacto Charpy | 23.0 °C | 11 J Show Material materials with Energía de impacto Charpy of 11 J | |
Estricción | 23.0 °C | 30 % Show Material materials with Estricción of 30 % | |
Límite elástico Rp 0,2 | 23.0 °C | 620 MPa Show Material materials with Límite elástico Rp 0,2 of 620 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 23.0 °C | 965 MPa Show Material materials with Resistencia a la tracción of 965 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.025 % Show Material materials with Aluminio of 0.025 % |
Azufre | 0.01 % Show Material materials with Azufre of 0.01 % |
Carbono | 0.2 - 0.25 % Show Material materials with Carbono of 0.2 - 0.25 % |
Cobalto | 0.2 % Show Material materials with Cobalto of 0.2 % |
Cobre | 0.15 % Show Material materials with Cobre of 0.15 % |
Cromo | 11 - 12.5 % Show Material materials with Cromo of 11 - 12.5 % |
Estaño | 0.02 % Show Material materials with Estaño of 0.02 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Manganeso | 0.5 - 1 % Show Material materials with Manganeso of 0.5 - 1 % |
Molibdeno | 0.9 - 1.25 % Show Material materials with Molibdeno of 0.9 - 1.25 % |
Niobio | 0.05 % Show Material materials with Niobio of 0.05 % |
Níquel | 0.5 - 1 % Show Material materials with Níquel of 0.5 - 1 % |
Silicona | 0.2 - 0.5 % Show Material materials with Silicona of 0.2 - 0.5 % |
Titanio | 0.03 % Show Material materials with Titanio of 0.03 % |
Vanadio | 0.2 - 0.3 % Show Material materials with Vanadio of 0.2 - 0.3 % |
Wolframio | 0.9 - 1.25 % Show Material materials with Wolframio of 0.9 - 1.25 % |