Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 163 - 217 [-] Show Material materials with Dureza Brinell of 163 - 217 [-] |
Elongación A50 | 20.0 °C | 18 % Show Material materials with Elongación A50 of 18 % |
Estricción | 20.0 °C | 45 % Show Material materials with Estricción of 45 % |
Resistencia a la tracción | 20.0 °C | 550 MPa Show Material materials with Resistencia a la tracción of 550 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 310 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 310 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % |
Carbono | 0.38 - 0.48 % Show Material materials with Carbono of 0.38 - 0.48 % |
Cromo | 0.8 - 1.2 % Show Material materials with Cromo of 0.8 - 1.2 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.75 - 1.1 % Show Material materials with Manganeso of 0.75 - 1.1 % |
Molibdeno | 0.15 - 0.25 % Show Material materials with Molibdeno of 0.15 - 0.25 % |
Silicona | 0.15 - 0.4 % Show Material materials with Silicona of 0.15 - 0.4 % |
Vanadio | 0.1 % Show Material materials with Vanadio of 0.1 % |