General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Elongación A50 | 23.0 °C | 20 % Show Material materials with Elongación A50 of 20 % | |
Límite elástico | 23.0 °C | 230 MPa Show Material materials with Límite elástico of 230 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 23.0 °C | 310 MPa Show Material materials with Resistencia a la tracción of 310 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.04 % Show Material materials with Azufre of 0.04 % |
Carbono | 0.2 % Show Material materials with Carbono of 0.2 % |
Cobre | 0.25 % Show Material materials with Cobre of 0.25 % |
Cromo | 0.15 % Show Material materials with Cromo of 0.15 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 1.35 % Show Material materials with Manganeso of 1.35 % |
Molibdeno | 0.06 % Show Material materials with Molibdeno of 0.06 % |
Niobio | 8E-3 % Show Material materials with Niobio of 8E-3 % |
Níquel | 0.2 % Show Material materials with Níquel of 0.2 % |
Titanio | 0.03 % Show Material materials with Titanio of 0.03 % |
Vanadio | 8E-3 % Show Material materials with Vanadio of 8E-3 % |