Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 8.8 g/cm³ Show Material materials with Densidad of 8.8 g/cm³ | Typical for Nickel Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Nickel Steel |
Dureza Vickers | 23.0 °C | 130 [-] Show Material materials with Dureza Vickers of 130 [-] | |
Elongación A50 | 23.0 °C | 38 % Show Material materials with Elongación A50 of 38 % | |
Hardness, Rockwell Superficial 15-T | 23.0 °C | 82 [-] Show Material materials with Hardness, Rockwell Superficial 15-T of 82 [-] | |
Límite elástico Rp 0,2 | 23.0 °C | 220 MPa Show Material materials with Límite elástico Rp 0,2 of 220 MPa | |
Módulo de cizallamiento | 23.0 °C | 76 GPa Show Material materials with Módulo de cizallamiento of 76 GPa | Typical for Nickel Steel |
Módulo elástico | 23.0 °C | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Nickel Steel |
Resistencia a la tracción | 23.0 °C | 500 MPa Show Material materials with Resistencia a la tracción of 500 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 456 J/(kg·K) Show Material materials with Calor específico of 456 J/(kg·K) | Typical for Nickel Steel |
Conductividad térmica | 23.0 °C | 10 - 50 W/(m·K) Show Material materials with Conductividad térmica of 10 - 50 W/(m·K) | Typical for Nickel Steel |
Temperatura de fusión | 1316 - 1595 °C Show Material materials with Temperatura de fusión of 1316 - 1595 °C | Typical for Nickel Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.01 % Show Material materials with Azufre of 0.01 % |
Carbono | 0.05 % Show Material materials with Carbono of 0.05 % |
Cobalto | 0.5 % Show Material materials with Cobalto of 0.5 % |
Cobre | 0.3 % Show Material materials with Cobre of 0.3 % |
Cromo | 0.3 % Show Material materials with Cromo of 0.3 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.8 % Show Material materials with Manganeso of 0.8 % |
Molibdeno | 0.3 % Show Material materials with Molibdeno of 0.3 % |
Níquel | 43.5 - 46.5 % Show Material materials with Níquel of 43.5 - 46.5 % |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % |