Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers | 20.0 °C | 320 [-] Show Material materials with Dureza Vickers of 320 [-] |
Elongación A50 | 20.0 °C | 2 % Show Material materials with Elongación A50 of 2 % |
Hardness, Rockwell Superficial 15-N | 20.0 °C | 78 [-] Show Material materials with Hardness, Rockwell Superficial 15-N of 78 [-] |
Chemical properties
Property | Value |
---|---|
Azufre | 0.01 % Show Material materials with Azufre of 0.01 % |
Carbono | 0.05 % Show Material materials with Carbono of 0.05 % |
Cobalto | 0.5 % Show Material materials with Cobalto of 0.5 % |
Cobre | 4 - 6 % Show Material materials with Cobre of 4 - 6 % |
Cromo | 2 - 3 % Show Material materials with Cromo of 2 - 3 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Manganeso | 1.5 % Show Material materials with Manganeso of 1.5 % |
Molibdeno | 0.5 % Show Material materials with Molibdeno of 0.5 % |
Níquel | 75 - 78 % Show Material materials with Níquel of 75 - 78 % |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % |