Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A50 | 23.0 °C | 16.5 - 30 % Show Material materials with Elongación A50 of 16.5 - 30 % |
Límite elástico | 23.0 °C | 275 MPa Show Material materials with Límite elástico of 275 MPa |
Resistencia a la tracción | 23.0 °C | 485 MPa Show Material materials with Resistencia a la tracción of 485 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.035 % Show Material materials with Azufre of 0.035 % |
Carbono | 0.35 % Show Material materials with Carbono of 0.35 % |
Cobre | 0.4 % Show Material materials with Cobre of 0.4 % |
Cromo | 0.4 % Show Material materials with Cromo of 0.4 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 0.29 - 1.06 % Show Material materials with Manganeso of 0.29 - 1.06 % |
Molibdeno | 0.15 % Show Material materials with Molibdeno of 0.15 % |
Níquel | 0.4 % Show Material materials with Níquel of 0.4 % |
Silicona | 0.1 % Show Material materials with Silicona of 0.1 % |
Vanadio | 0.08 % Show Material materials with Vanadio of 0.08 % |