General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 20.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Manganese Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Manganese Steel |
Dureza Brinell | 20.0 °C | 149 - 207 [-] Show Material materials with Dureza Brinell of 149 - 207 [-] | |
Elongación A50 | 20.0 °C | 22 % Show Material materials with Elongación A50 of 22 % | |
Energía de impacto Charpy | 20.0 °C | 41 J Show Material materials with Energía de impacto Charpy of 41 J | |
Estricción | 20.0 °C | 40 % Show Material materials with Estricción of 40 % | |
Módulo elástico | 20.0 °C | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Manganese Steel |
Resistencia a la tracción | 20.0 °C | 415 MPa Show Material materials with Resistencia a la tracción of 415 MPa | |
Yield Strength Rp0.2, short transverse | 20.0 °C | 290 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 290 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 510 - 553 J/(kg·K) Show Material materials with Calor específico of 510 - 553 J/(kg·K) | Typical for Manganese Steel |
Coeficiente de dilatación térmica | 20.0 °C | 1.33E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.33E-5 1/K | Typical for Manganese Steel |
Conductividad térmica | 20.0 °C | 14 - 16 W/(m·K) Show Material materials with Conductividad térmica of 14 - 16 W/(m·K) | Typical for Manganese Steel |
Temperatura de fusión | 1382 - 1529 °C Show Material materials with Temperatura de fusión of 1382 - 1529 °C | Typical for Manganese Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % |
Carbono | 0.07 % Show Material materials with Carbono of 0.07 % |
Cobre | 0.4 % Show Material materials with Cobre of 0.4 % |
Cromo | 0.3 % Show Material materials with Cromo of 0.3 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 1.85 - 2.2 % Show Material materials with Manganeso of 1.85 - 2.2 % |
Molibdeno | 0.25 - 0.35 % Show Material materials with Molibdeno of 0.25 - 0.35 % |
Niobio | 0.06 - 0.1 % Show Material materials with Niobio of 0.06 - 0.1 % |
Níquel | 0.4 % Show Material materials with Níquel of 0.4 % |
Silicona | 0.15 % Show Material materials with Silicona of 0.15 % |
Vanadio | 0.05 % Show Material materials with Vanadio of 0.05 % |