General
Property | Value | Comment |
---|---|---|
Densidad | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coeficiente de Poisson | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel | |||
Dureza Brinell | 149.0 - 207.0 [-] Show Material materials with Dureza Brinell of 149.0 - 207.0 [-] | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging | |
Energía de impacto Charpy | 41.0 J Show Material materials with Energía de impacto Charpy of 41.0 J | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging | |
Estricción | 40.0 % Show Material materials with Estricción of 40.0 % | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging | |
Módulo elástico | 190.0 - 210.0 GPa Show Material materials with Módulo elástico of 190.0 - 210.0 GPa | Typical for Steel | |||
Resistencia a la tracción | 415.0 MPa Show Material materials with Resistencia a la tracción of 415.0 MPa | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Azufre | 0.02 Show Material materials with Azufre of 0.02 | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging |
Carbono | 0.2 Show Material materials with Carbono of 0.2 | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging |
Cobre | 0.4 Show Material materials with Cobre of 0.4 | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging |
Cromo | 1.5 - 2.0 % Show Material materials with Cromo of 1.5 - 2.0 % | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging |
Fósforo | 0.02 Show Material materials with Fósforo of 0.02 | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging |
Manganeso | 0.2 - 0.4 % Show Material materials with Manganeso of 0.2 - 0.4 % | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging |
Molibdeno | 0.4 - 0.6 % Show Material materials with Molibdeno of 0.4 - 0.6 % | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging |
Niobio | 0.02 Show Material materials with Niobio of 0.02 | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging |
Níquel | 2.8 - 3.9 % Show Material materials with Níquel of 2.8 - 3.9 % | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging |
Silicona | 0.35 Show Material materials with Silicona of 0.35 | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging |
Vanadio | 0.05 Show Material materials with Vanadio of 0.05 | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging |