Mecánica
Chemical properties
Property | Value |
---|---|
Azufre | 0.04 % Show Material materials with Azufre of 0.04 % |
Carbono | 0.35 - 0.75 % Show Material materials with Carbono of 0.35 - 0.75 % |
Cromo | 15 - 19 % Show Material materials with Cromo of 15 - 19 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 2 % Show Material materials with Manganeso of 2 % |
Molibdeno | 0.5 % Show Material materials with Molibdeno of 0.5 % |
Níquel | 33 - 37 % Show Material materials with Níquel of 33 - 37 % |
Silicona | 2.5 % Show Material materials with Silicona of 2.5 % |