Mecánica
Chemical properties
Property | Value |
---|---|
Azufre | 0.04 % Show Material materials with Azufre of 0.04 % |
Carbono | 0.35 - 0.75 % Show Material materials with Carbono of 0.35 - 0.75 % |
Cromo | 17 - 21 % Show Material materials with Cromo of 17 - 21 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 2 % Show Material materials with Manganeso of 2 % |
Molibdeno | 0.5 % Show Material materials with Molibdeno of 0.5 % |
Níquel | 37 - 41 % Show Material materials with Níquel of 37 - 41 % |
Silicona | 2.5 % Show Material materials with Silicona of 2.5 % |