Mecánica
Property | Temperature | Value |
---|---|---|
Resistencia a la tracción | 20.0 °C | 415 MPa Show Material materials with Resistencia a la tracción of 415 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.04 % Show Material materials with Azufre of 0.04 % |
Carbono | 0.35 - 0.75 % Show Material materials with Carbono of 0.35 - 0.75 % |
Cromo | 10 - 14 % Show Material materials with Cromo of 10 - 14 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 2 % Show Material materials with Manganeso of 2 % |
Molibdeno | 0.5 % Show Material materials with Molibdeno of 0.5 % |
Níquel | 58 - 62 % Show Material materials with Níquel of 58 - 62 % |
Silicona | 2.5 % Show Material materials with Silicona of 2.5 % |