Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A50 | 23.0 °C | 15 % Show Material materials with Elongación A50 of 15 % |
Estricción | 23.0 °C | 45 % Show Material materials with Estricción of 45 % |
Límite elástico | 23.0 °C | 415 MPa Show Material materials with Límite elástico of 415 MPa |
Resistencia a la tracción | 23.0 °C | 585 MPa Show Material materials with Resistencia a la tracción of 585 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.2 % Show Material materials with Carbono of 0.2 % |
Cromo | 1 - 1.5 % Show Material materials with Cromo of 1 - 1.5 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 0.5 - 0.9 % Show Material materials with Manganeso of 0.5 - 0.9 % |
Molibdeno | 0.9 - 1.2 % Show Material materials with Molibdeno of 0.9 - 1.2 % |
Silicona | 0.2 - 0.6 % Show Material materials with Silicona of 0.2 - 0.6 % |
Vanadio | 0.2 - 0.35 % Show Material materials with Vanadio of 0.2 - 0.35 % |