Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 131 - 183 [-] Show Material materials with Dureza Brinell of 131 - 183 [-] |
Resistencia a la tracción | 23.0 °C | 172 MPa Show Material materials with Resistencia a la tracción of 172 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.12 % Show Material materials with Azufre of 0.12 % |
Carbono | 3 % Show Material materials with Carbono of 3 % |
Cobre | 5.5 - 7.5 % Show Material materials with Cobre of 5.5 - 7.5 % |
Cromo | 1.5 - 2.5 % Show Material materials with Cromo of 1.5 - 2.5 % |
Manganeso | 0.5 - 1.5 % Show Material materials with Manganeso of 0.5 - 1.5 % |
Níquel | 13.5 - 17.5 % Show Material materials with Níquel of 13.5 - 17.5 % |
Silicona | 1 - 2.8 % Show Material materials with Silicona of 1 - 2.8 % |