General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.15 g/cm³ Show Material materials with Densidad of 7.15 g/cm³ | Typical for Grey Cast Iron |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.21 [-] Show Material materials with Coeficiente de Poisson of 0.21 [-] | Typical for Grey Cast Iron |
Dureza Brinell | 23.0 °C | 99 - 124 [-] Show Material materials with Dureza Brinell of 99 - 124 [-] | |
Módulo de cizallamiento | 23.0 °C | 41 GPa Show Material materials with Módulo de cizallamiento of 41 GPa | Typical for Cast Iron |
Módulo elástico | 23.0 °C | 92.4 GPa Show Material materials with Módulo elástico of 92.4 GPa | Typical for Grey Cast Iron |
Resistencia a la tracción | 23.0 °C | 138 MPa Show Material materials with Resistencia a la tracción of 138 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 460 J/(kg·K) Show Material materials with Calor específico of 460 J/(kg·K) | Typical for Grey Cast Iron |
Coeficiente de dilatación térmica | 23.0 °C | 1.1E-5 - 1.5E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.1E-5 - 1.5E-5 1/K | Typical for Grey Cast Iron |
Conductividad térmica | 23.0 °C | 20 - 80 W/(m·K) Show Material materials with Conductividad térmica of 20 - 80 W/(m·K) | Typical for Grey Cast Iron |
Temperatura de fusión | 1127 - 1204 °C Show Material materials with Temperatura de fusión of 1127 - 1204 °C | Typical for Grey Cast Iron |
Chemical properties
Property | Value |
---|---|
Azufre | 0.12 % Show Material materials with Azufre of 0.12 % |
Carbono | 2.4 % Show Material materials with Carbono of 2.4 % |
Cobre | 0.5 % Show Material materials with Cobre of 0.5 % |
Cromo | 0.1 % Show Material materials with Cromo of 0.1 % |
Manganeso | 0.5 - 1.5 % Show Material materials with Manganeso of 0.5 - 1.5 % |
Níquel | 34 - 36 % Show Material materials with Níquel of 34 - 36 % |
Silicona | 1 - 2 % Show Material materials with Silicona of 1 - 2 % |