General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 8.8 g/cm³ Show Material materials with Densidad of 8.8 g/cm³ | Typical for Nickel Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Nickel Steel |
Dureza Brinell | 23.0 °C | 139 - 202 [-] Show Material materials with Dureza Brinell of 139 - 202 [-] | |
Elongación A50 | 23.0 °C | 8 % Show Material materials with Elongación A50 of 8 % | |
Límite elástico Rp 0,2 | 23.0 °C | 210 MPa Show Material materials with Límite elástico Rp 0,2 of 210 MPa | |
Módulo de cizallamiento | 23.0 °C | 76 GPa Show Material materials with Módulo de cizallamiento of 76 GPa | Typical for Nickel Steel |
Módulo elástico | 23.0 °C | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Nickel Steel |
Resistencia a la tracción | 23.0 °C | 400 MPa Show Material materials with Resistencia a la tracción of 400 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 456 J/(kg·K) Show Material materials with Calor específico of 456 J/(kg·K) | Typical for Nickel Steel |
Conductividad térmica | 23.0 °C | 10 - 50 W/(m·K) Show Material materials with Conductividad térmica of 10 - 50 W/(m·K) | Typical for Nickel Steel |
Temperatura de fusión | 1316 - 1595 °C Show Material materials with Temperatura de fusión of 1316 - 1595 °C | Typical for Nickel Steel |
Chemical properties
Property | Value |
---|---|
Carbono | 3 % Show Material materials with Carbono of 3 % |
Cromo | 1.75 - 2.75 % Show Material materials with Cromo of 1.75 - 2.75 % |
Fósforo | 0.08 % Show Material materials with Fósforo of 0.08 % |
Manganeso | 0.7 - 1.25 % Show Material materials with Manganeso of 0.7 - 1.25 % |
Níquel | 18 - 22 % Show Material materials with Níquel of 18 - 22 % |