Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 131 - 193 [-] Show Material materials with Dureza Brinell of 131 - 193 [-] |
Elongación A50 | 20.0 °C | 10 % Show Material materials with Elongación A50 of 10 % |
Resistencia a la tracción | 20.0 °C | 380 MPa Show Material materials with Resistencia a la tracción of 380 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 210 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 210 MPa |
Chemical properties
Property | Value |
---|---|
Carbono | 2.3 % Show Material materials with Carbono of 2.3 % |
Cromo | 1.75 - 2.25 % Show Material materials with Cromo of 1.75 - 2.25 % |
Fósforo | 0.08 % Show Material materials with Fósforo of 0.08 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Níquel | 34 - 37 % Show Material materials with Níquel of 34 - 37 % |
Silicona | 4.9 - 5.5 % Show Material materials with Silicona of 4.9 - 5.5 % |