Mecánica
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.2 - 0.45 % Show Material materials with Carbono of 0.2 - 0.45 % |
Cromo | 23 - 28 % Show Material materials with Cromo of 23 - 28 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 2.5 % Show Material materials with Manganeso of 2.5 % |
Nitrógeno | 0.2 % Show Material materials with Nitrógeno of 0.2 % |
Níquel | 10 - 14 % Show Material materials with Níquel of 10 - 14 % |
Silicona | 1.75 % Show Material materials with Silicona of 1.75 % |