Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 0 - 235 [-] Show Material materials with Dureza Brinell of 0 - 235 [-] |
Dureza Rockwell C | 20.0 °C | 0 - 22 [-] Show Material materials with Dureza Rockwell C of 0 - 22 [-] |
Elongación A50 | 20.0 °C | 0 - 22 % Show Material materials with Elongación A50 of 0 - 22 % |
Estricción | 20.0 °C | 0 - 40 % Show Material materials with Estricción of 0 - 40 % |
Resistencia a la tracción | 20.0 °C | 0 - 620 MPa Show Material materials with Resistencia a la tracción of 0 - 620 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 0 - 450 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 0 - 450 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0 - 0.035 % Show Material materials with Azufre of 0 - 0.035 % |
Carbono | 0 - 0.3 % Show Material materials with Carbono of 0 - 0.3 % |
Cobre | 0 - 0.5 % Show Material materials with Cobre of 0 - 0.5 % |
Cromo | 0 - 0.35 % Show Material materials with Cromo of 0 - 0.35 % |
Fósforo | 0 - 0.04 % Show Material materials with Fósforo of 0 - 0.04 % |
Manganeso | 1 - 1.4 % Show Material materials with Manganeso of 1 - 1.4 % |
Molibdeno | 0.1 - 0.3 % Show Material materials with Molibdeno of 0.1 - 0.3 % |
Níquel | 0 - 0.5 % Show Material materials with Níquel of 0 - 0.5 % |
Silicona | 0 - 0.8 % Show Material materials with Silicona of 0 - 0.8 % |
Vanadio | 0 - 0.03 % Show Material materials with Vanadio of 0 - 0.03 % |
Wolframio | 0 - 0.1 % Show Material materials with Wolframio of 0 - 0.1 % |