Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A50 | 20.0 °C | 14 % Show Material materials with Elongación A50 of 14 % |
Estricción | 20.0 °C | 30 % Show Material materials with Estricción of 30 % |
Resistencia a la tracción | 20.0 °C | 825 MPa Show Material materials with Resistencia a la tracción of 825 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 655 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 655 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.035 % Show Material materials with Azufre of 0.035 % |
Boro | 0.4 % Show Material materials with Boro of 0.4 % |
Carbono | 0.55 % Show Material materials with Carbono of 0.55 % |
Cobre | 0.1 % Show Material materials with Cobre of 0.1 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 0.8 - 1.1 % Show Material materials with Manganeso of 0.8 - 1.1 % |
Molibdeno | 0.2 - 0.3 % Show Material materials with Molibdeno of 0.2 - 0.3 % |
Níquel | 0.03 % Show Material materials with Níquel of 0.03 % |
Silicona | 0.6 % Show Material materials with Silicona of 0.6 % |